Instead of sulfuric acid treatment, try alkali washing instead using weak sodium hydroxide solution (around 5 - 10%). The amount of solution to the oil maybe around 8%. Mix for about 1 hour before settling out the water. dry the oil well before acid clay bleaching. good luck!