Dear amitss
At the given pressure conditions there is no issue with Expanded only T-TS joint.
What are your temperature conditions? Was the exchanger fixed tubesheet one like AEM or BEM ?
If the diff in shell and tube ave temperatures is more may be thermal expansion is culprite?