Just to add to my above post,
Kindly note that the AD merkblatt also requires additional testing at the product manufacturing stage.
I.e it mandates hot tensile test to be performed for all materials at the maximum design temperature or 300 deg C (if design temperature is not mentioned) so that the actual yield strength at design temperature is verified.

Thus the allowable stress based on yield strength which is considered during design can be safely used.